2. Technical requirement
2.1 Outside appearance
The board material should be flat and smooth, no bubble, no wrinkle, no crackle, free from other defects, such as a scrape, compress, dirt spot, and uneven of color, allow a few of color spots.
| PERFORMANCE | UNIT | TEST METHOD | INDEX VALUE |
| Vertical layer direction bending strength | MPa | GB/T5130 section 5.1 | ≥ 152 |
| Parallel layer direction compact strength (Simple strut-beam) | KJ/m2 | GB/T5130 section 5.5 | ≥ 25 |
| Parallel layer direction compact strength (Suspended arm beam method) | KJ/m2 | GB/T5130 section 5.5 | ≥ 26 |
| Relative dielectric factor (1 MHZ below) | | GB/T5130 section 6.2 | ≤ 5.5 |
| Mediate loss factor(1 MHZ below) | | GB/T5130 section 6.2 | ≤ 0.04 |
| Vertical layer direction electric strength at (90±2)°C oil. | MV/m | GB/T5130 section 6.1 | Refer to table 2 |
| Parallel layer direction breakdown voltage at (90±2)°C oil. | kV | GB/T5130 section 6.1 | ≥ 15 |
| Insulation resistance after water dipping | Ω | GB/T5130 section 6.3 | ≥ 3.0 × 108 |
| Density | g/cm3 | GB/T5130 section 8.1 | 1.7 - 2.0 |
| Water absorption | mg | GB/T5130 section 8.2 | Refer to table 3 |
Table 2: Vertical layer direction electric strength
| AVERAGE THICKNESS MM | ELECTRIC STRENGTH MV/MM | AVERAGE THICKNESS MM | ELECTRIC STRENGTH MV/MM | AVERAGE THICKNESS MM | ELECTRIC STRENGTH MV/MM |
| 0.4 | ≥ 16.9 | 1.0 | ≥ 14.2 | 2.2 | ≥ 11.4 |
| 0.5 | ≥ 16.1 | 1.2 | ≥ 13.7 | 2.4 | ≥ 11.1 |
| 0.6 | ≥ 15.6 | 1.4 | ≥ 13.2 | 2.5 | ≥ 10.9 |
| 0.7 | ≥ 15.2 | 1.6 | ≥ 12.7 | 2.6 | ≥ 10.8 |
| 0.8 | ≥ 14.8 | 1.8 | ≥ 12.2 | 2.8 | ≥ 10.5 |
| 0.9 | ≥ 14.5 | 2.0 | ≥ 11.8 | 3.0 | ≥ 10.2 |
Table 3: Water absorption
| SAMPLE THICKNESS MEAN VALUE (D) MM | WATER ABSORPTION MG | SAMPLE THICKNESS MEAN VALUE (D) MM | WATER ABSORPTION MG |
| 0.4 <= d ≤ 1.0 | ≤ 18 | 6.0 < d ≤ 10 | ≤ 30 |
| 1.0 < d <= 2.0 | ≤ 20 | 10.0 < d≤ 20 | ≤ 34 |
| 2.0 < d <= 3.0 | ≤ 25 | 2.0 < d ≤ 25 | ≤ 52 |
| 3.0 < d <= 6.0 | | | |